effect of the microstructure and distribution of the second phase on the stress corrosion cracking of biomedical mg-zn-zr-xsr alloys

Clicks: 223
ID: 170162
2018
Article Quality & Performance Metrics
Overall Quality Improving Quality
0.0 /100
Combines engagement data with AI-assessed academic quality
AI Quality Assessment
Not analyzed
Abstract
The stress corrosion cracking (SCC) properties of the bi-directional forged (BDF) Mg-4Zn-0.6Zr-xSr (ZK40-xSr, x = 0, 0.4, 0.8, 1.2, 1.6 wt %) alloys were studied by the slow strain rate tensile (SSRT) testing in modified simulated body fluid (m-SBF). The average grain size of the BDF alloys were approximately two orders of magnitude smaller than those of the as-cast alloys. However, grain refinement increased the hydrogen embrittlement effect, leading to a higher SCC susceptibility in the BDF ZK40-0/0.4Sr alloys. Apart from the grain refinements effect, the forging process also changed the distribution of second phase from the net-like shape along the grain boundary to a uniformly isolated island shape in the BDF alloys. The SCC susceptibility of the BDF ZK40-1.2/1.6Sr alloys were lower than those of the as-cast alloys. The change of distribution of the second phase suppressed the adverse effect of Sr on the SCC susceptibility in high Sr–containing magnesium alloys. The results indicated the stress corrosion behavior of magnesium alloys was related to the average grain size of matrix and the distribution and shape of the second phase.
Reference Key
chen2018materialseffect Use this key to autocite in the manuscript while using SciMatic Manuscript Manager or Thesis Manager
Authors ;Lianxi Chen;Yinying Sheng;Xiaojian Wang;Xueyang Zhao;Hui Liu;Wei Li
Journal Nature Materials
Year 2018
DOI
10.3390/ma11040551
URL
Keywords

Citations

No citations found. To add a citation, contact the admin at info@scimatic.org

No comments yet. Be the first to comment on this article.