structural effects of metallic chromium on its electrochemical behavior

Clicks: 337
ID: 170225
2007
Article Quality & Performance Metrics
Overall Quality
Not rated
Combines reader engagement with the AI quality analysis. This article has not been analysed, so there is no overall score — reader engagement is measured and shown alongside.
AI Quality Assessment
Not analyzed
Readership in this journal
Steady

Ranked #10 of 151 articles by views in meditsinskaia radiologiia

Most read Least read

Bar heights use a square-root scale. Only the 120 most-read articles are drawn; the journal has 151 in total.

Mint this article as an NFT
Not yet minted

Create a permanent, verifiable on-chain record of this article on the Scimatic Network. The NFT is held in your Journament account, and you can withdraw it to your own wallet at any time.

5 SUSD one-off · no wallet required
Abstract
Chromium dissolution in aqueous sulfuric acid solution of pH 1 was studied electrochemically on chromium electrodes with different crystallographic structures. A slow potentiodynamic method was used for the electrochemical measurements in deaerated solutions (purgedwith nitrogen),while the Cr(III) ions in the solution after the corrosion were determined by atomic absorption spectrometry. Three electrode materials with a very dominant crystallite orientation resembling single crystal structures (i.e., 111 and 110) confirmed by the electron backscattering diffraction (EBSD), were used in the experiments. The (111) structures were somewhat more active electrochemically (both anodic and cathodic) than the (110) structure. However, Cr electrochemically deposited in standard plating bath, assumed from literature data to has also the (111) structure, was more than 4 times active for anodic dissolution and, by the same number, less active for cathodic hydrogen evolution. The concentrations of Cr(III) ions determined in the solution after definite times of corrosion of all the materials showed almost two times larger dissolution rates than observed electrochemically by three different electrochemical methods (Wagner–Traud, Stern–Geary, electrochemical impedance spectroscopy). This is explained by the simultaneous occurrence of potential independent chemical dissolution of Cr, by a direct reaction of metallic Cr with H2O molecules, proposed a long time ago by Kolotyrkin and coworkers.
Reference Key
radmilovic2007journalstructural Use this key to autocite in the manuscript while using SciMatic Manuscript Manager or Thesis Manager
Authors ;VELIMIR RADMILOVIC;JOVAN P. POPIC;DRAGUTIN M. DRAZIC;BORE JEGDIC
Journal meditsinskaia radiologiia
Year 2007
DOI
DOI not found
URL
Keywords

Citations

No citations found. To add a citation, contact the admin at info@scimatic.org

No comments yet. Be the first to comment on this article.