wear and corrosion performances of new friction materials for automotive industry

Clicks: 310
ID: 158559
2012
Article Quality & Performance Metrics
Overall Quality
Not rated
Combines reader engagement with the AI quality analysis. This article has not been analysed, so there is no overall score — reader engagement is measured and shown alongside.
AI Quality Assessment
Not analyzed
Readership in this journal
Popular

Ranked #16 of 98 articles by views in journal of the formosan medical association = taiwan yi zhi

Most read Least read

Bar heights use a square-root scale.

Mint this article as an NFT
Not yet minted

Create a permanent, verifiable on-chain record of this article on the Scimatic Network. The NFT is held in your Journament account, and you can withdraw it to your own wallet at any time.

5 SUSD one-off · no wallet required
Abstract
In this study, after a NiCr bond layer was deposited on a pearlitic, grey cast iron rotor disc of the kind used in a production passenger car (Toyota Corolla 1600 cc), Cr3C2-NiCr and Al2O3-TiO2powders were sprayed using High Velocity Oxygen Fuel(HVOF) and plasma spray processes, respectively. The discs were subjected to cosmetic corrosion test according to SAE J2334 test standard. Additionally, wear tests were carried out using a reciprocating wear tester by rubbing a 10 mm diameter Al2O3 ball on the specimens machined from rotor discs in salt solution. It was found that the Cr3C2-NiCr coating (HSCN) sprayed using HVOF method exhibited highest hardness and highest corrosion and wear resistances.
Reference Key
samur2012metalurgijawear Use this key to autocite in the manuscript while using SciMatic Manuscript Manager or Thesis Manager
Authors ;R. Samur;A. Demir
Journal journal of the formosan medical association = taiwan yi zhi
Year 2012
DOI
DOI not found
URL
Keywords

Citations

No citations found. To add a citation, contact the admin at info@scimatic.org

No comments yet. Be the first to comment on this article.