Analysis of self-heating of thermally assisted spin-transfer torque magnetic random access memory
Clicks: 230
ID: 87890
2016
Article Quality & Performance Metrics
Overall Quality
Not rated
Combines reader engagement with the AI quality analysis. This
article has not been analysed, so there is no overall score —
reader engagement is measured and shown alongside.
Reader Engagement
Popular Article
30.0
/100
230 views
31 readers
AI Quality Assessment
Not analyzed
Readership in this journal
PopularRanked #21 of 44 articles by views in beilstein journal of nanotechnology
Most read
Least read
Bar heights use a square-root scale.
Mint this article as an NFT
Not yet mintedCreate a permanent, verifiable on-chain record of this article on the Scimatic Network. The NFT is held in your Journament account, and you can withdraw it to your own wallet at any time.
5
SUSD
one-off · no wallet required
Abstract
Thermal assistance has been shown to significantly reduce the required operation power for spin torque transfer magnetic random access memory (STT-MRAM). Proposed heating methods include modified material stack compositions that result in increased self-heating or external heat sources. In this work we analyze the self-heating process of a standard perpendicular magnetic anisotropy STT-MRAM device through numerical simulations in order to understand the relative contributions of Joule, thermoelectric Peltier and Thomson, and tunneling junction heating. A 2D rotationally symmetric numerical model is used to solve the coupled electro-thermal equations including thermoelectric effects and heat absorbed or released at the tunneling junction. We compare self-heating for different common passivation materials, positive and negative electrical current polarity, and different device thermal anchoring and boundaries resistance configurations. The variations considered are found to result in significant differences in maximum temperatures reached. Average increases of 3 K, 10 K, and 100 K for different passivation materials, positive and negative polarity, and different thermal anchoring configurations, respectively, are observed. The highest temperatures, up to 424 K, are obtained for silicon dioxide as the passivation material, positive polarity, and low thermal anchoring with thermal boundary resistance configurations. Interestingly it is also found that due to the tunneling heat, Peltier effect, device geometry, and numerous interfacial layers around the magnetic tunnel junction (MTJ), most of the heat is dissipated on the lower potential side of the magnetic junction. This asymmetry in heating, which has also been observed experimentally, is important as thermally assisted switching requires heating of the free layer specifically and this will be significantly different for the two polarity operations, set and reset.
| Reference Key |
deschenes2016analysisbeilstein
Use this key to autocite in the manuscript while using
SciMatic Manuscript Manager or Thesis Manager
|
|---|---|
| Authors | Deschenes, Austin;Muneer, Sadid;Akbulut, Mustafa;Gokirmak, Ali;Silva, Helena; |
| Journal | beilstein journal of nanotechnology |
| Year | 2016 |
| DOI |
DOI not found
|
| URL | |
| Keywords |
Citations
No citations found. To add a citation, contact the admin at info@scimatic.org
Comments
No comments yet. Be the first to comment on this article.