A new model of trajectory in eddy current separation for recovering spent lithium iron phosphate batteries.
Clicks: 214
ID: 41090
2019
Article Quality & Performance Metrics
Overall Quality
Not rated
Combines reader engagement with the AI quality analysis. This
article has not been analysed, so there is no overall score —
reader engagement is measured and shown alongside.
Reader Engagement
Steady Performance
64.3
/100
214 views
169 readers
Trending
AI Quality Assessment
Not analyzed
Readership in this journal
SteadyRanked #101 of 145 articles by views in waste management (new york, ny)
Most read
Least read
Bar heights use a square-root scale. Only the 120 most-read articles are drawn; the journal has 145 in total.
Mint this article as an NFT
Not yet mintedCreate a permanent, verifiable on-chain record of this article on the Scimatic Network. The NFT is held in your Journament account, and you can withdraw it to your own wallet at any time.
5
SUSD
one-off · no wallet required
Abstract
Eddy current separation (ECS) is an environment-friendly technology for separating nonferrous metallic particles whose size was from 2 mm to 10 mm. No wastes are generated in ECS. ECS quality of nonferrous metals from solid wastes is rather low in the production practice of spent lithium iron phosphate (LFP) batteries recovering. Repeating separation even manual sorting is required in the production. The traditional method of falling point prediction based on eddy current mechanics uses equivalent acceleration to replace separation motion curves. These curves have low precision and are unsuitable for predicting the motion trajectory of small particle size of sorted materials. In this work, eddy current separation of positive and negative plates in a crushed product of spent lithium iron phosphate battery is used as an example to establish the force and kinematics models of different materials in the eddy current separation. An iterative method, rather than average speed method, is used to improve the accuracy of the model. Displacement interval replaces disengagement angle as a separating index to improve the model's intuitiveness and practical guidance. In the range of 2-20 mm, test results are consistent with simulation results. The copper and aluminium foils at a magnetic roller speed of 800r/min can be separated to a maximum particle size ratio of 1.72, and the maximum particle size ratio of copper and positive electrode sheets can be large. This paper provided an environmental-friendly and effective technology for separating nonferrous metals from crushed spent LFP batteries.
| Reference Key |
bi2019awaste
Use this key to autocite in the manuscript while using
SciMatic Manuscript Manager or Thesis Manager
|
|---|---|
| Authors | Bi, Haijun;Zhu, Huabing;Zu, Lei;Bai, Yuxuan;Gao, Song;Gao, Yong; |
| Journal | waste management (new york, ny) |
| Year | 2019 |
| DOI |
S0956-053X(19)30567-7
|
| URL | |
| Keywords | Keywords not found |
Citations
No citations found. To add a citation, contact the admin at info@scimatic.org
Comments
No comments yet. Be the first to comment on this article.