removal of so42− from li2co3 by recrystallization in na2co3 solution

Clicks: 184
ID: 252029
2018
Article Quality & Performance Metrics
Overall Quality
Not rated
Combines reader engagement with the AI quality analysis. This article has not been analysed, so there is no overall score — reader engagement is measured and shown alongside.
AI Quality Assessment
Not analyzed
Readership in this journal
Emerging

Ranked #69 of 88 articles by views in turk kardiyoloji dernegi arsivi

Most read Least read

Bar heights use a square-root scale.

Mint this article as an NFT
Not yet minted

Create a permanent, verifiable on-chain record of this article on the Scimatic Network. The NFT is held in your Journament account, and you can withdraw it to your own wallet at any time.

5 SUSD one-off · no wallet required
Abstract
Li2CO3 with high purity is an important raw material for the fabrication of lithium rechargeable batteries. This paper reports a facile recrystallization way to produce Li2CO3 with high purity from commercial Li2CO3 containing 0.8 wt % of SO42− by the treatment of the commercial Li2CO3 in Na2CO3 solution. The increase of temperature from 30 °C to 90 °C favored the recrystallization of Li2CO3 in Na2CO3 solution and promoted the removal of SO42− adsorbed or doped on/in the commercial Li2CO3. The content of SO42− in Li2CO3 decreased to 0.08 wt % after the treatment of the commercial Li2CO3 in 1.0 mol·L−1 Na2CO3 solution at 90 °C for 10.0 h.
Reference Key
cai2018crystalsremoval Use this key to autocite in the manuscript while using SciMatic Manuscript Manager or Thesis Manager
Authors ;Wei Cai;Ruosong Chen;Yurong Yang;Meigui Yi;Lan Xiang
Journal turk kardiyoloji dernegi arsivi
Year 2018
DOI
10.3390/cryst8010019
URL
Keywords

Citations

No citations found. To add a citation, contact the admin at info@scimatic.org

No comments yet. Be the first to comment on this article.