Abstract
The purpose of this study was to evaluate the effect of five primers [Super-Bond C&B Monomer (SB), Clearfil Ceramic Primer, Alloy Primer, M.L. Primer, and AZ Primer] and two undercoating opaque resins [Super-Bond C&B (S-opaque) and Ceramage Pre-opaque (C-opaque)] on the bonding of a resin composite veneering material to a ceria-stabilized tetragonal zirconia polycrystals/alumina nanocomposite (Ce-TZP/Al2O3). Disk-shaped specimens of Ce-TZP/Al2O3 were sandblasted with alumina and primed. The undercoating opaque resins and resin composites were subsequently applied to the specimen, and then light cured. After 5000 thermocycles at 4°C and 60°C, shear bond strengths were determined. Data were analyzed using analysis of variance, Tukey–Kramer honest significant difference test, and Student t test (n = 10, α = 0.05). With the exception of SB/S-opaque, all S-opaque groups exhibited significantly higher bond strengths than C-opaque groups. The use of S-opaque resin is recommended when veneering frameworks made of Ce-TZP/Al2O3.
| Reference Key |
kamada2017journalevaluation
Use this key to autocite in the manuscript while using
SciMatic Manuscript Manager or Thesis Manager
|
|---|---|
| Authors | ;Kohji Kamada;Yohsuke Taira;Ikuya Watanabe;Takashi Sawase |
| Journal | world academy of science, engineering and technology |
| Year | 2017 |
| DOI |
10.1016/j.jds.2016.05.004
|
| URL | |
| Keywords |
Citations
No citations found. To add a citation, contact the admin at info@scimatic.org
Comments
No comments yet. Be the first to comment on this article.