effects of solution treating on microstructural and mechanical properties of a heavily deformed new biocompatible ti–nb–zr–fe alloy

Clicks: 377
ID: 181521
2018
Article Quality & Performance Metrics
Overall Quality
Not rated
Combines reader engagement with the AI quality analysis. This article has not been analysed, so there is no overall score — reader engagement is measured and shown alongside.
AI Quality Assessment
Not analyzed
Readership in this journal
Steady

Ranked #20 of 136 articles by views in seminars in cancer biology

Most read Least read

Bar heights use a square-root scale. Only the 120 most-read articles are drawn; the journal has 136 in total.

Mint this article as an NFT
Not yet minted

Create a permanent, verifiable on-chain record of this article on the Scimatic Network. The NFT is held in your Journament account, and you can withdraw it to your own wallet at any time.

5 SUSD one-off · no wallet required
Abstract
The effects of heavy cold plastic deformation by rolling on microstructural features and mechanical properties of Ti–25Nb–6Zr–1.7Fe (wt %) biocompatible alloy (TNZF) were studied. After a preliminary alloy processing, a heavy plastic deformation by cold-rolling (CR) with a total relative degree of plastic deformation of 90% (equivalent plastic strain, ε = 2.42) and a subsequent solution heat treatment (CR+ST) at 900 °C for 0.6 ks/water quenching were applied and then investigated. The CR and CR+ST states have microstructures consisting of mixtures of β-Ti phases and α″-Ti. The alloy in CR state shows a pronounced deformation texture, with highly deformed and elongated β-Ti grains, exhibiting internal highly fragmented areas, with shear lines at about 45° and a sub-micron/nanocrystalline fine dispersed α″-Ti phase. The alloy in CR+ST state has completely recrystallized equiaxed polyhedral β-Ti grains, with average grain size close to 52 μm and a sub-micron/nanocrystalline fine dispersed α″-Ti phase. Recorded mechanical properties, for both CR and CR+ST states, show quite similar values for the yield strength (σ0.2), ultimate tensile strength (σUTS) and Vickers microhardness (HV0.1) for CR state (σ0.2 = 603 MPa, σUTS = 1282 MPa and 287 HV0.1) in comparison with CR+ST state (σ0.2 = 598 MPa, σUTS = 1256 MPa and 256 HV0.1). Values for the modulus of elasticity (E) are lower (E = 72 GPa for CR state and E = 61 GPa for CR+ST state) than those for conventional biocompatible alloys (E ~ 110 GPa).
Reference Key
cojocaru2018metalseffects Use this key to autocite in the manuscript while using SciMatic Manuscript Manager or Thesis Manager
Authors
Journal seminars in cancer biology
Year 2018
DOI
10.3390/met8050297
URL
Keywords

Citations

No citations found. To add a citation, contact the admin at info@scimatic.org

No comments yet. Be the first to comment on this article.