Improvement of Gold Leaching from a Refractory Gold Concentrate Calcine by Separate Pretreatment of Coarse and Fine Size Fractions
Clicks: 364
ID: 86719
2017
Article Quality & Performance Metrics
Overall Quality
Not rated
Combines reader engagement with the AI quality analysis. This
article has not been analysed, so there is no overall score —
reader engagement is measured and shown alongside.
Reader Engagement
Popular Article
30.0
/100
364 views
54 readers
AI Quality Assessment
Not analyzed
Readership in this journal
PopularRanked #6 of 27 articles by views in minerals
Most read
Least read
Bar heights use a square-root scale.
Mint this article as an NFT
Not yet mintedCreate a permanent, verifiable on-chain record of this article on the Scimatic Network. The NFT is held in your Journament account, and you can withdraw it to your own wallet at any time.
5
SUSD
one-off · no wallet required
Abstract
A total gold extraction of 70.2% could only be reached via direct cyanidation from a refractory As-, S- and C-bearing gold concentrate calcine, and the gold extraction varied noticeably with different size fractions. The reasons for unsatisfactory gold extraction from the calcine were studied through analyses of chemical composition, chemical phase and SEM-EDS of different sizes of particles. It was found that a significant segregation of compositions occurred during the grinding of gold ore before flotation. As a result, for the calcine obtained after oxidative roasting, the encapsulation of gold by iron oxides was easily engendered in finer particles, whilst in coarser particles the gold encapsulation by silicates was inclined to occur likely due to melted silicates blocking the porosity of particles. The improvement of gold leaching from different size fractions was further investigated through pretreatments with alkali washing, acid pickling or sulfuric acid curing-water leaching. Finally, a novel process was recommended and the total gold extraction from the calcine could be increased substantially to 93.6% by the purposeful pretreatment with alkali washing for the relatively coarse size fraction (+37 μm) and sulfuric acid curing–water leaching for the fine size fraction (−37 μm).
| Reference Key |
li2017improvementminerals
Use this key to autocite in the manuscript while using
SciMatic Manuscript Manager or Thesis Manager
|
|---|---|
| Authors | Li, Qian;Zhang, Yan;Liu, Xiaoliang;Xu, Bin;Yang, Yongbin;Jiang, Tao; |
| Journal | minerals |
| Year | 2017 |
| DOI |
DOI not found
|
| URL | |
| Keywords |
Citations
No citations found. To add a citation, contact the admin at info@scimatic.org
Comments
No comments yet. Be the first to comment on this article.