QUALITY OF SAWN TIMBER DRYING OF Eucalyptus dunnii

Clicks: 337
ID: 63915
2009
Article Quality & Performance Metrics
Overall Quality
Not rated
Combines reader engagement with the AI quality analysis. This article has not been analysed, so there is no overall score — reader engagement is measured and shown alongside.
AI Quality Assessment
Not analyzed
Readership in this journal
Popular

Ranked #6 of 12 articles by views in ciência florestal

Most read Least read

Bar heights use a square-root scale.

Mint this article as an NFT
Not yet minted

Create a permanent, verifiable on-chain record of this article on the Scimatic Network. The NFT is held in your Journament account, and you can withdraw it to your own wallet at any time.

5 SUSD one-off · no wallet required
Abstract

In the present study, the behaviour of Eucalyptus dunnii wood drying in a conventional pilot kiln was evaluated, using three drying schedules. Each drying schedule had an initial vaporization (presteaming) of 3 hours after one hour of initial warming and an intermediate vaporization of 5 hours for the collapse recovery when the wood was at 17% of humidity. The results show that among the used drying schedule only the schedule regarded as the mildest presented a good result in terms of dry wood quality. Among the discovered defects, there were 37,5% of collapse, 35% of cupping and 10% of split. Hoviever, though from this total only 15% of the collapse and cupping were regarded as strong defects.

Reference Key
severo2009qualitycincia Use this key to autocite in the manuscript while using SciMatic Manuscript Manager or Thesis Manager
Authors Severo, Elias Taylor Durgante;
Journal ciência florestal
Year 2009
DOI
DOI not found
URL
Keywords

Citations

No citations found. To add a citation, contact the admin at info@scimatic.org

No comments yet. Be the first to comment on this article.