Surface-oxygen vacancy defect-promoted electron-hole separation of defective tungsten trioxide ultrathin nanosheets and their enhanced solar-driven photocatalytic performance.

Clicks: 247
ID: 42652
2019
Article Quality & Performance Metrics
Overall Quality
Not rated
Combines reader engagement with the AI quality analysis. This article has not been analysed, so there is no overall score — reader engagement is measured and shown alongside.
AI Quality Assessment
Not analyzed
Readership in this journal
Steady

Ranked #83 of 128 articles by views in Journal of colloid and interface science

Most read Least read

Bar heights use a square-root scale. Only the 120 most-read articles are drawn; the journal has 128 in total.

Mint this article as an NFT
Not yet minted

Create a permanent, verifiable on-chain record of this article on the Scimatic Network. The NFT is held in your Journament account, and you can withdraw it to your own wallet at any time.

5 SUSD one-off · no wallet required
Abstract
Defective WO ultrathin surface-engineered nanosheets are fabricated by a solvothermal and low-temperature surface hydrogenation reduction strategy. The obtained defective WO ultrathin nanosheets with thicknesses of ∼4 nm possess a relatively large surface area of ∼25 m g. After surface engineering, the bandgap is narrowed to ∼2.48 eV due to the presence of surface oxygen vacancies, which further enhance the visible light absorption. The defective WO ultrathin nanosheets exhibit excellent solar-driven photocatalytic degradation performance for the complete degradation of the highly-toxic metribuzin herbicide (∼100%). The first-order rate constant (k) of the defective WO ultrathin nanosheets is ∼3 times higher than that of the pristine one. This can be ascribed to the formation of suitable surface-oxygen vacancy defects that promote the separation of photogenerated electron-hole pairs, and the two-dimensional ultrathin structure facilitating the surface engineering as well as furnishing a large number of surface active sites. Moreover, the defective WO ultrathin nanosheets exhibit high stability because the photocatalytic activity remains almost unchanged after 10 cycles, making them favorable for practical applications. This work offers new insights into the fabrication of other high-performance ultrathin nanosheet oxide photocatalysts for environmental applications.
Reference Key
wu2019surfaceoxygenjournal Use this key to autocite in the manuscript while using SciMatic Manuscript Manager or Thesis Manager
Authors Wu, Jiaxing;Qiao, Panzhe;Li, Haoze;Ren, Liping;Xu, Yachao;Tian, Guohui;Li, Mingxia;Pan, Kai;Zhou, Wei;
Journal Journal of colloid and interface science
Year 2019
DOI
S0021-9797(19)31039-2
URL
Keywords Keywords not found

Citations

No citations found. To add a citation, contact the admin at info@scimatic.org