Ethanol as Dentin Pretreatment on the Bonding Performance of a Two-Step Etch-and-Rinse Adhesive: An In Vivo Study.
Clicks: 293
ID: 34223
2019
Article Quality & Performance Metrics
Overall Quality
Not rated
Combines reader engagement with the AI quality analysis. This
article has not been analysed, so there is no overall score —
reader engagement is measured and shown alongside.
Reader Engagement
Steady Performance
79.5
/100
293 views
208 readers
Trending
AI Quality Assessment
Not analyzed
Readership in this journal
SteadyRanked #10 of 15 articles by views in european journal of dentistry
Most read
Least read
Bar heights use a square-root scale.
Mint this article as an NFT
Not yet mintedCreate a permanent, verifiable on-chain record of this article on the Scimatic Network. The NFT is held in your Journament account, and you can withdraw it to your own wallet at any time.
5
SUSD
one-off · no wallet required
Abstract
The aim of this study was to evaluate the use of 70 vol.% ethanol as a dentin pretreatment on the bond strength (BS) of a two-step etch-and-rinse adhesive.Resin composite Class I restorations were clinically bonded to acid-etched dentin of human sound third molars using Adper Single Bond 2 (SB, 3M ESPE) and randomly divided into two major groups: dentin saturated with water (control) or 70 vol.% ethanol (ethanol). The teeth were divided into two subgroups: immediately extracted and tested after 24 hours and extraction after 18 months. Bonded teeth (Adper SB 2) were cut into resin-dentin sticks that were tested by microtensile BS, and the failure mode was thereafter evaluated.Data were statistically analyzed using two-way analysis of variance and Holm-Sidak test (α = 0.05). Additional bonded resin-dentin slabs from each group were examined under light microscopy (LM) using the Masson's trichrome staining technique.The lowest BS was obtained by ethanol pretreated dentin after aging, while other groups presented similar BS. The LM analysis showed the presence of resin-sparse collagen fibrils in groups examined immediately (24 hours) and the presence of several gaps due to collagen degradation at the interfaces of ethanol pretreated aged specimens (18 months).The use of 70 vol.% ethanol in dentin before the application of a two-step etch-and-rinse adhesive should be avoided once it resulted in a significant drop on the BS.
| Reference Key |
silva2019ethanoleuropean
Use this key to autocite in the manuscript while using
SciMatic Manuscript Manager or Thesis Manager
|
|---|---|
| Authors | Silva, Francisco Cláudio Fernandes Alves;Feitosa, Victor Pinheiro;Saboia, Vicente de Paulo Aragão; |
| Journal | european journal of dentistry |
| Year | 2019 |
| DOI |
10.1055/s-0039-1696584
|
| URL | |
| Keywords | Keywords not found |
Citations
No citations found. To add a citation, contact the admin at info@scimatic.org
Comments
No comments yet. Be the first to comment on this article.