Synthesis and Properties of Ethylene/propylene and Ethylene/propylene/5-ethylidene-2-norbornene Copolymers Obtained on -Et(2-MeInd)ZrMe/Isobutylaluminium Aryloxide Catalytic Systems.
Clicks: 159
ID: 276556
2023
Article Quality & Performance Metrics
Overall Quality
Not rated
Combines reader engagement with the AI quality analysis. This
article has not been analysed, so there is no overall score —
reader engagement is measured and shown alongside.
Reader Engagement
Emerging Content
30.0
/100
159 views
23 readers
AI Quality Assessment
Not analyzed
Readership in this journal
EmergingRanked #178 of 250 articles by views in Polymers
Most read
Least read
Bar heights use a square-root scale. Only the 120 most-read articles are drawn; the journal has 250 in total.
Mint this article as an NFT
Not yet mintedCreate a permanent, verifiable on-chain record of this article on the Scimatic Network. The NFT is held in your Journament account, and you can withdraw it to your own wallet at any time.
5
SUSD
one-off · no wallet required
Abstract
Ethylene/propylene (E/P) and ethylene/propylene/5-ethylidene-2-norbornene (E/P/ENB) copolymers were obtained on -Et(2-MeInd)ZrMe activated by a number of isobutylaluminium aryloxides: (2,6-BuPhO-)AlBu (1-DTBP) (2,6-Bu,4-Me-PhO-)AlBu (1-BHT), (2,4,6-BuPhO-)AlBu (1-TTBP), (2,6-Bu,4-Me-PhO-)AlBu (2-BHT), (2,6-BuPhO-)2AlBu (2-DTBP), [(2-Me,6-Bu-CHO)AlBu] (1-MTBP), [(2,6-Ph-PhO)AlBu] (1-DPP). This study shows how the structure of an activator influences catalytic activity and polymer properties, such as the copolymer composition, molecular weight characteristics, and thermophysical and mechanical properties. It has been shown that both the introduction of a bulky substituent in the para-position of the aryloxy group and the additional aryloxy group in the structure of an activator lead to a significant decrease in activity of the catalytic system in all studied copolymerization processes. Moreover, activation by bulkier aryloxides leads to lower levels of comonomer insertion and gives rise to higher molecular weight polymers. Broad or multiple endothermic peaks with different values of melting points are observed on the DSC curves of the copolymers obtained with different catalytic systems. The DSC of the thermally fractionated samples makes it possible to reveal the heterogeneity of the copolymer microstructure, which manifests itself in the presence of a set of lamellar crystallites of different thickness. The results also present the mechanical properties of the copolymers, such as the tensile strength (σ), elongation at break (ε), and engineering strain (EL). The synthesized E/P and E/P/ENB copolymers contain about 1-4 wt.% of the sterically hindered phenols obtained in situ as a residue of the hydrolyzed activators in the course of reaction quenching. This determines the increased thermooxidative stability of the copolymers.
| Reference Key |
faingold2023synthesispolymers
Use this key to autocite in the manuscript while using
SciMatic Manuscript Manager or Thesis Manager
|
|---|---|
| Authors | Faingol'd, Evgeny E;Saratovskikh, Stanislav L;Panin, Andrei N;Babkina, Olga N;Zharkov, Igor V;Kapasharov, Artur T;Bubnova, Maria L;Shilov, Gennady V;Bravaya, Natalia M; |
| Journal | Polymers |
| Year | 2023 |
| DOI |
487
|
| URL | |
| Keywords |
Citations
No citations found. To add a citation, contact the admin at info@scimatic.org
Comments
No comments yet. Be the first to comment on this article.