Textile Based Electrochromic Cells Prepared with PEDOT: PSS and Gelled Electrolyte

Clicks: 198
ID: 267607
2020
Article Quality & Performance Metrics
Overall Quality
Not rated
Combines reader engagement with the AI quality analysis. This article has not been analysed, so there is no overall score — reader engagement is measured and shown alongside.
AI Quality Assessment
Not analyzed
Readership in this journal
Emerging

Ranked #1,343 of 1,694 articles by views in sensors

Most read Least read

Bar heights use a square-root scale. Only the 120 most-read articles are drawn; the journal has 1,694 in total.

Mint this article as an NFT
Not yet minted

Create a permanent, verifiable on-chain record of this article on the Scimatic Network. The NFT is held in your Journament account, and you can withdraw it to your own wallet at any time.

5 SUSD one-off · no wallet required
Abstract
Electrochromic devices can act as passive displays. They change their color when a low voltage is applied. Flexible and bendable hybrid textile-film electrochromic devices with poly-3,4-ethylenedioxythiophene polystyrene sulfonate (PEDOT:PSS) were prepared on polyethylene polyethylene terephthalate (PEPES) membranes using a spray coating technique. The electrolyte consisted of a gelatin glycerol mixture as host matrix and calcium chloride. Titanium dioxide was used as an ion storage layer and a carbon containing dispersion was used for the counter electrode on a polyester rip-stop fabric. The sheet resistance of PEDOT:PSS on PEPES was 500 Ohm/sq. A 5 × 5 electrochromic matrix with individually addressable pixels was successfully designed and assembled. The switching time of the pixels was 2 s at a voltage of 2.0 V directly after assembling. The use of titanium dioxide as ion storage also increased the contrast of the dark-blue reduced electrochromic layer. Coloration was not self-sustaining. The PEDOT:PSS layer needed a constant low voltage of at least 0.5 V to sustain in the dark-blue reduced state. The switching time increased with time. After 12 months the switching time was ~4 s at a voltage of 2.8 V. The addition of glycerol into the electrolyte extended the lifetime of a non-encapsulated textile electrochromic cell, because moisture is retained in the electrolyte. Charge carriers can be transported into and out of the electrochromic layer.
Reference Key
graßmann2020sensorstextile Use this key to autocite in the manuscript while using SciMatic Manuscript Manager or Thesis Manager
Authors Carsten Graßmann;Maureen Mann;Lieva Van Langenhove;Anne Schwarz-Pfeiffer;Graßmann, Carsten;Mann, Maureen;Van Langenhove, Lieva;Schwarz-Pfeiffer, Anne;
Journal sensors
Year 2020
DOI
10.3390/s20195691
URL
Keywords

Citations

No citations found. To add a citation, contact the admin at info@scimatic.org

No comments yet. Be the first to comment on this article.