repair of the orbital wall fractures in rabbit animal model using nanostructured hydroxyapatite-based implant

Clicks: 95
ID: 235846
2016
Article Quality & Performance Metrics
Overall Quality
Not rated
Combines reader engagement with the AI quality analysis. This article has not been analysed, so there is no overall score — reader engagement is measured and shown alongside.
AI Quality Assessment
Not analyzed
Readership in this journal
Steady

Ranked #130 of 133 articles by views in progress in neuro-psychopharmacology & biological psychiatry

Most read Least read

Bar heights use a square-root scale. Only the 120 most-read articles are drawn; the journal has 133 in total.

Mint this article as an NFT
Not yet minted

Create a permanent, verifiable on-chain record of this article on the Scimatic Network. The NFT is held in your Journament account, and you can withdraw it to your own wallet at any time.

5 SUSD one-off · no wallet required
Abstract
Cellular uptake and cytotoxicity of nanostructured hydroxyapatite (nanoHAp) are dependent on its physical parameters. Therefore, an understanding of both surface chemistry and morphology of nanoHAp is needed in order to be able to anticipate its in vivo behavior. The aim of this paper is to characterize an engineered nanoHAp in terms of physico-chemical properties, biocompatibility, and its capability to reconstitute the orbital wall fractures in rabbits. NanoHAp was synthesized using a high pressure hydrothermal method and characterized by physico-chemical, structural, morphological, and optical techniques. X-ray diffraction revealed HAp crystallites of 21 nm, while Scanning Electron Microscopy (SEM) images showed spherical shapes of HAp powder. Mean particle size of HAp measured by DLS technique was 146.3 nm. Biocompatibility was estimated by the effect of HAp powder on the adhesion and proliferation of mesenchymal stem cells (MSC) in culture. The results showed that cell proliferation on powder-coated slides was between 73.4% and 98.3% of control cells (cells grown in normal culture conditions). Computed tomography analysis of the preformed nanoHAp implanted in orbital wall fractures, performed at one and two months postoperative, demonstrated the integration of the implants in the bones. In conclusion, our engineered nanoHAp is stable, biocompatible, and may be safely considered for reconstruction of orbital wall fractures.
Reference Key
gradinaru2016nanomaterialsrepair Use this key to autocite in the manuscript while using SciMatic Manuscript Manager or Thesis Manager
Authors ;Sinziana Gradinaru;Laura Madalina Popescu;Roxana Mioara Piticescu;Sabina Zurac;Radu Ciuluvica;Alexandrina Burlacu;Raluca Tutuianu;Sorina-Nicoleta Valsan;Adrian Mihail Motoc;Liliana Mary Voinea
Journal progress in neuro-psychopharmacology & biological psychiatry
Year 2016
DOI
10.3390/nano6010011
URL
Keywords

Citations

No citations found. To add a citation, contact the admin at info@scimatic.org

No comments yet. Be the first to comment on this article.