crack-configuration analysis of metal conductive track embedded in stretchable elastomer
Clicks: 5
ID: 235137
2018
Article Quality & Performance Metrics
Overall Quality
Not rated
Combines reader engagement with the AI quality analysis. This
article has not been analysed, so there is no overall score —
reader engagement is measured and shown alongside.
Reader Engagement
Emerging Content
1.2
/100
5 views
4 readers
AI Quality Assessment
Not analyzed
Readership in this journal
EmergingRanked #113 of 115 articles by views in chemistryopen
Most read
Least read
Bar heights use a square-root scale.
Mint this article as an NFT
Not yet mintedCreate a permanent, verifiable on-chain record of this article on the Scimatic Network. The NFT is held in your Journament account, and you can withdraw it to your own wallet at any time.
5
SUSD
one-off · no wallet required
Abstract
This paper reports the analysis of the crack configuration of a stretched metal conductive track that is embedded in a stretchable elastomer. The factor determining the crack configurations is analyzed by modeling as well as experiments. The modeling analysis indicates that the crack configuration is determined by the ratio of the elongation stiffness of the track and elastomer, and is classified into two types: multiple-crack growth and single-crack growth. When the track stiffness is considerably lower than the elastomer stiffness, multiple-crack growth type occurs; in the opposite case, single-crack growth type occurs. Hence, to verify the modeling analysis, metal conductive tracks with different thicknesses are fabricated, and the cracks are studied with respect to the crack width, number of cracks, and crack propagation speed. In this study, two conventional metal-track shapes are studied: straight-shaped tracks with track thickness of 0.04–1.17 µm, and wave-shaped tracks with track thickness of 2–10 µm. For straight-shaped tracks, multiple-crack growth type occurred, when the track thickness was 0.04 µm, and the crack configuration gradually changed to a single crack, with the increase in the track thickness. For wave-shaped tracks with track thickness of 2–10 µm, only single-crack growth type occurred; however, the crack propagation speed decreased and the maximum stretchability of the track increased, with the increase in the track thickness.
| Reference Key |
koshi2018micromachinescrack-configuration
Use this key to autocite in the manuscript while using
SciMatic Manuscript Manager or Thesis Manager
|
|---|---|
| Authors | ;Tomoya Koshi;Eiji Iwase |
| Journal | chemistryopen |
| Year | 2018 |
| DOI |
10.3390/mi9030130
|
| URL | |
| Keywords | Keywords not found |
Citations
No citations found. To add a citation, contact the admin at info@scimatic.org
Comments
No comments yet. Be the first to comment on this article.