recovery of cerium dioxide from spent glass-polishing slurry and its utilization as a reactive sorbent for fast degradation of toxic organophosphates

Clicks: 213
ID: 218442
2015
Article Quality & Performance Metrics
Overall Quality
Not rated
Combines reader engagement with the AI quality analysis. This article has not been analysed, so there is no overall score — reader engagement is measured and shown alongside.
AI Quality Assessment
Not analyzed
Readership in this journal
Steady

Ranked #67 of 254 articles by views in bulletin of the korean chemical society

Most read Least read

Bar heights use a square-root scale. Only the 120 most-read articles are drawn; the journal has 254 in total.

Mint this article as an NFT
Not yet minted

Create a permanent, verifiable on-chain record of this article on the Scimatic Network. The NFT is held in your Journament account, and you can withdraw it to your own wallet at any time.

5 SUSD one-off · no wallet required
Abstract
The recovery of cerium (and possibly other rare earth elements) from the spent glass-polishing slurries is rather difficult because of a high resistance of polishing-grade cerium oxide toward common digestion agents. It was shown that cerium may be extracted from the spent polishing slurries by leaching with strong mineral acids in the presence of reducing agents; the solution may be used directly for the preparation of a ceria-based reactive sorbent. A mixture of concentrated nitric acid and hydrogen peroxide was effective in the digestion of partially dewatered glass-polishing slurry. After the removal of undissolved particles, cerous carbonate was precipitated by gaseous NH3 and CO2. Cerium oxide was prepared by a thermal decomposition of the carbonate precursor in an open crucible and tested as reactive sorbent for the degradation of highly toxic organophosphate compounds. The samples annealed at the optimal temperature of approximately 400°C exhibited a good degradation efficiency toward the organophosphate pesticide fenchlorphos and the nerve agents soman and VX. The extraction/precipitation procedure recovers approximately 70% of cerium oxide from the spent polishing slurry. The presence of minor amounts of lanthanum does not disturb the degradation efficiency.
Reference Key
jano2015advancesrecovery Use this key to autocite in the manuscript while using SciMatic Manuscript Manager or Thesis Manager
Authors ;Pavel Janoš;Pavel Kuráň;Jakub Ederer;Martin Šťastný;Luboš Vrtoch;Martin Pšenička;Jiří Henych;Karel Mazanec;Miroslav Skoumal
Journal bulletin of the korean chemical society
Year 2015
DOI
10.1155/2015/241421
URL
Keywords

Citations

No citations found. To add a citation, contact the admin at info@scimatic.org

No comments yet. Be the first to comment on this article.