raman spectroscopic study of as-deposited and exfoliated defected graphene grown on (001) si substrates by cvd

Clicks: 259
ID: 205075
2017
Article Quality & Performance Metrics
Overall Quality
Not rated
Combines reader engagement with the AI quality analysis. This article has not been analysed, so there is no overall score — reader engagement is measured and shown alongside.
AI Quality Assessment
Not analyzed
Readership in this journal
Steady

Ranked #81 of 150 articles by views in acs nano

Most read Least read

Bar heights use a square-root scale. Only the 120 most-read articles are drawn; the journal has 150 in total.

Mint this article as an NFT
Not yet minted

Create a permanent, verifiable on-chain record of this article on the Scimatic Network. The NFT is held in your Journament account, and you can withdraw it to your own wallet at any time.

5 SUSD one-off · no wallet required
Abstract
We present here results on a Raman spectroscopic study of the deposited defected graphene on Si substrates by chemical vapor deposition (thermal decomposition of acetone). The graphene films are not deposited on the (001) Si substrate directly but on two types of interlayers of mixed phases unintentionally deposited on the substrates: а diamond-like carbon (designated here as DLC) and amorphous carbon (designated here as αC) are dominated ones. The performed thorough Raman spectroscopic study of as-deposited as well as exfoliated specimens by two different techniques using different excitation wavelengths (488, 514, and 613 nm) as well as polarized Raman spectroscopy establishes that the composition of the designated DLC layers varies with depth: the initial layers on the Si substrate consist of DLC, nanodiamond species, and C70 fullerenes while the upper ones are dominated by DLC with an occasional presence of C70 fullerenes. The αC interlayer is dominated by turbostratic graphite and contains a larger quantity of C70 than the DLC-designated interlayers. The results of polarized and unpolarized Raman spectroscopic studies of as-grown and exfoliated graphene films tend to assume that single- to three-layered defected graphene is deposited on the interlayers. It can be concluded that the observed slight upshift of the 2D band as well as the broadening of 2D band should be related to the strain and doping.
Reference Key
milenov2017journalraman Use this key to autocite in the manuscript while using SciMatic Manuscript Manager or Thesis Manager
Authors ;T. I. Milenov;E. Valcheva;V. N. Popov
Journal acs nano
Year 2017
DOI
10.1155/2017/3495432
URL
Keywords

Citations

No citations found. To add a citation, contact the admin at info@scimatic.org

No comments yet. Be the first to comment on this article.