spectroscopic studies of the behavior of eu3+ on the luminescence of cadmium tellurite glasses
Clicks: 212
ID: 205017
2015
Article Quality & Performance Metrics
Overall Quality
Not rated
Combines reader engagement with the AI quality analysis. This
article has not been analysed, so there is no overall score —
reader engagement is measured and shown alongside.
Reader Engagement
Popular Article
30.0
/100
212 views
46 readers
AI Quality Assessment
Not analyzed
Readership in this journal
PopularRanked #109 of 150 articles by views in acs nano
Most read
Least read
Bar heights use a square-root scale. Only the 120 most-read articles are drawn; the journal has 150 in total.
Mint this article as an NFT
Not yet mintedCreate a permanent, verifiable on-chain record of this article on the Scimatic Network. The NFT is held in your Journament account, and you can withdraw it to your own wallet at any time.
5
SUSD
one-off · no wallet required
Abstract
The effect of europium doping on the photoluminescence of ZnO-CdO-TeO2 glasses is analyzed. TeO2-based glasses are of high interest as hosts for laser glasses. The Eu-doped oxide glasses were prepared by the conventional melt-quenching method. Five different concentrations of europium nitrate hexahydrate that varied from 0.3 to 1.5 mol% were used. SEM observations revealed the formation of zinc aluminate spinel and disperse droplets of liquid-liquid phase separation in the glasses. X-Ray diffraction reveals the amorphous structure of the fabricated glasses. FT-IR and Raman spectra show the presence of TeO4 and TeO3+1/TeO3 units that conform with the glass matrix. Raman spectra evidenced a band located at 1556 cm−1 that can be related to interstitial molecular oxygen in the glass matrix. Photoluminescence of the glasses showed light emission due to the following europiumtransitions from its D52, D51, and D50 levels to its F7J manifolds: D52→F70 (468 nm), D52→F72 (490 nm), D52→F73 (511 nm), D51→F71 (536 nm), D51→F72 (554 nm), D50→F70 (579.5 nm), D50→F71 (592 nm), D50→F72 (613 nm), D50→F73 (652 nm), and D50→F74 (490 nm). The estimated decay time, τ, was 0.4 ms for all the glasses.
| Reference Key |
garca-amaya2015journalspectroscopic
Use this key to autocite in the manuscript while using
SciMatic Manuscript Manager or Thesis Manager
|
|---|---|
| Authors | ;I. V. García-Amaya;Ma. E. Zayas;J. Alvarado-Rivera;E. Álvarez;S. A. Gallardo-Heredia;G. A. Limón;R. Lozada-Morales;J. Ma. Rincón |
| Journal | acs nano |
| Year | 2015 |
| DOI |
10.1155/2015/478329
|
| URL | |
| Keywords |
Citations
No citations found. To add a citation, contact the admin at info@scimatic.org
Comments
No comments yet. Be the first to comment on this article.