prevention of burn-on defect on surface of hydroturbine blade casting of ultra-low-carbon refining stainless steel

Clicks: 169
ID: 183785
2008
Free PDF
Article Quality & Performance Metrics
Overall Quality
Not rated
Combines reader engagement with the AI quality analysis. This article has not been analysed, so there is no overall score — reader engagement is measured and shown alongside.
AI Quality Assessment
Not analyzed
Readership in this journal
Popular

Ranked #30 of 41 articles by views in bioconjugate chemistry

Most read Least read

Bar heights use a square-root scale.

Mint this article as an NFT
Not yet minted

Create a permanent, verifiable on-chain record of this article on the Scimatic Network. The NFT is held in your Journament account, and you can withdraw it to your own wallet at any time.

5 SUSD one-off · no wallet required
Abstract
The burn-on sand is common surface defect encountered in CO2-cured silicate-bonded sand casting of hydroturbine blade of ultra-low-carbon martensitic stainless steel, its feature, causes and prevention measures are presented in this paper. Experiments showed that the burn-on defect is caused by oxidization of chromium in the molten steel at high temperature and can be effectively eliminated by using chromium-corundum coating.
Reference Key
ling2008chinaprevention Use this key to autocite in the manuscript while using SciMatic Manuscript Manager or Thesis Manager
Authors
Journal bioconjugate chemistry
Year 2008
DOI
DOI not found
URL
Keywords Keywords not found

Citations

No citations found. To add a citation, contact the admin at info@scimatic.org

No comments yet. Be the first to comment on this article.