practical contributions to the study of resistance assemblies made with warp knits

Clicks: 297
ID: 174838
2014
Article Quality & Performance Metrics
Overall Quality
Not rated
Combines reader engagement with the AI quality analysis. This article has not been analysed, so there is no overall score — reader engagement is measured and shown alongside.
AI Quality Assessment
Not analyzed
Readership in this journal
Popular

Ranked #8 of 16 articles by views in hemijska industrija

Most read Least read

Bar heights use a square-root scale.

Mint this article as an NFT
Not yet minted

Create a permanent, verifiable on-chain record of this article on the Scimatic Network. The NFT is held in your Journament account, and you can withdraw it to your own wallet at any time.

5 SUSD one-off · no wallet required
Abstract
Based on the principle that a body to be obtained by sewing the material to provide resistance and the like in the stitching assembly, the experimental study of which developed resistance is compared with the resistance materials to effectively assembled by the assembly line. The experimental values resistance for assemblies were obtained in the testing for resistance to sliding stitch ASTM D 434 using Tinius Olsen HK5T test type machine. The assembly strength was determined for warp knitted fabric and satin charmeuse, made of poly-filamentary wires and mono-filament polyester and polyamide. Resistance assembling is one of the major determinants of the quality of the stitching. It is defined as "the tensile strength or friction." Tenacity stitching seam rupture is the force recorded at its weakest point. Seam abrasion resistance is the number of cycles required friction mesh destruction of seam. It can be said that the strength of the used assembly, the seam 301 is achieved by, in most of the cases, lower resistance knitted studied. In these cases, the primary findings presented, it is clear that the assembly is not appropriate in terms of reliability and maintainability of the product. Such a situation requires a first step to change the type (class) of stitch used. Another way to remedy the deficiencies could be using a sewing thread with a lower finesse or strength in grain, especially in the upper loop of wire used in the study-specific.
Reference Key
2014annalspractical Use this key to autocite in the manuscript while using SciMatic Manuscript Manager or Thesis Manager
Authors ;OANA Ioan-Pavel ;OANA Dorina
Journal hemijska industrija
Year 2014
DOI
DOI not found
URL
Keywords

Citations

No citations found. To add a citation, contact the admin at info@scimatic.org

No comments yet. Be the first to comment on this article.