evaluation of load-deflection properties of fiber-reinforced composites and its comparison with stainless steel wires
Clicks: 328
ID: 172851
2014
Article Quality & Performance Metrics
Overall Quality
Not rated
Combines reader engagement with the AI quality analysis. This
article has not been analysed, so there is no overall score —
reader engagement is measured and shown alongside.
Reader Engagement
Steady Performance
69.9
/100
328 views
232 readers
Trending
AI Quality Assessment
Not analyzed
Readership in this journal
SteadyRanked #18 of 59 articles by views in Mycoses
Most read
Least read
Bar heights use a square-root scale.
Mint this article as an NFT
Not yet mintedCreate a permanent, verifiable on-chain record of this article on the Scimatic Network. The NFT is held in your Journament account, and you can withdraw it to your own wallet at any time.
5
SUSD
one-off · no wallet required
Abstract
Background: The aim of this study was to evaluate the response of common sized fiber-reinforced composites (FRCs) to different deflections due to bending forces and comparing it with stainless steel (SS) wires.
Materials and Methods: In this experimental study, two FRC groups with 0.75 mm and 1.2 mm diameters (Everstick Ortho, Stick Tech, Finland) and three SS groups with 0.016 × 0.022 inch, 0.0215 × 0.028 inch and 0.7 mm diameters (3M Uniteck, Monrovia, California, USA) were tested. Each group contained 10 samples that were tested according to a three point bending test. Each group was tested at deflections of 0.5, 1 and 1.5 mm and the data was analyzed using the repeated measure ANOVA by SPSS software (Statistical Package for the Social Sciences, IBM SPSS, Inc. in Chicago, Illinois, USA). P < 0.05 was considered as significant.
Results: The highest recorded load belonged to the 1.2 mm FRC and after that 0.7 mm SS wire, 0.75 mm FRC, 0.0215 × 0.028 inch SS wire and finally 0.016 × 0.022 inch SS wire. The 0.7 mm SS wire and 0.75 mm FRC were compared as retainers and the results showed the 0.7 mm SS wire showed significantly higher load compared with 0.75 mm FRC (P < 0.05). The 1.2 mm FRC had significantly higher load compared to 0.0215 × 0.028 inch and 0.016 × 0.022 inch SS wires (P < 0.05).
Conclusion: The results showed that the 1.2 mm FRC group had significantly higher load compared to SS wires and other FRC groups under the 0.5, 1 and 1.5 mm deflections. Therefore, it can be suggested that FRC can be used as an esthetic replacement for SS wires for active and passive purposes in orthodontics.
| Reference Key |
alavi2014dentalevaluation
Use this key to autocite in the manuscript while using
SciMatic Manuscript Manager or Thesis Manager
|
|---|---|
| Authors | ;Shiva Alavi;Tayebe Mamavi |
| Journal | Mycoses |
| Year | 2014 |
| DOI |
DOI not found
|
| URL | |
| Keywords |
Citations
No citations found. To add a citation, contact the admin at info@scimatic.org
Comments
No comments yet. Be the first to comment on this article.