evaluation of the cool-down behaviour of iter fw beryllium tiles for an early failure detection

Clicks: 208
ID: 154749
2016
Article Quality & Performance Metrics
Overall Quality
Not rated
Combines reader engagement with the AI quality analysis. This article has not been analysed, so there is no overall score — reader engagement is measured and shown alongside.
AI Quality Assessment
Not analyzed
Readership in this journal
Popular

Ranked #24 of 25 articles by views in american business law journal

Most read Least read

Bar heights use a square-root scale.

Mint this article as an NFT
Not yet minted

Create a permanent, verifiable on-chain record of this article on the Scimatic Network. The NFT is held in your Journament account, and you can withdraw it to your own wallet at any time.

5 SUSD one-off · no wallet required
Abstract
The design of the first wall in ITER foresees several hundred thousand beryllium tiles, which are bonded to the water-cooled CuCrZr supporting structure. Due to the nature of a Tokamak reactor this bonding is faced to thermal fatigue. Since the failure of a single tile might already have a major impact on the operability of ITER, comprehensive high heat flux tests are performed on prototypes prior to the acceptance of manufacturing procedures. For a deeper understanding of the temperature curves, which were and will be measured by IR devices of these first wall prototypes, thermo-mechanical FEM simulations shall demonstrate the possibilities of an early bonding failure detection. Hereby, the maximum temperatures for each cycle as well as the cool-down behaviour are the input data.
Reference Key
weber2016nuclearevaluation Use this key to autocite in the manuscript while using SciMatic Manuscript Manager or Thesis Manager
Authors
Journal american business law journal
Year 2016
DOI
10.1016/j.nme.2016.08.009
URL
Keywords

Citations

No citations found. To add a citation, contact the admin at info@scimatic.org

No comments yet. Be the first to comment on this article.