Behavior of the Steel T91 under Multi Axial Loading in Contact with Liquid and Solid Pb
Clicks: 241
ID: 112432
2017
Article Quality & Performance Metrics
Overall Quality
Not rated
Combines reader engagement with the AI quality analysis. This
article has not been analysed, so there is no overall score —
reader engagement is measured and shown alongside.
Reader Engagement
Popular Article
30.0
/100
241 views
23 readers
AI Quality Assessment
Not analyzed
Readership in this journal
PopularRanked #42 of 66 articles by views in metals
Most read
Least read
Bar heights use a square-root scale.
Mint this article as an NFT
Not yet mintedCreate a permanent, verifiable on-chain record of this article on the Scimatic Network. The NFT is held in your Journament account, and you can withdraw it to your own wallet at any time.
5
SUSD
one-off · no wallet required
Abstract
In this work, the conditions for the occurrence of Liquid Metal Embrittlement (LME) in the ferritic-martensitic steel T91 in contact with lead, Pb, were examined. Slow tensile tests with notched specimens revealed that in a temperature range close to the melting point of Pb, the steel is sensitive to LME (350–400 °C) and to Solid Metal Induced Embrittlement (SMIE) (300 °C). The cracking was stimulated by wetting (using a chemical flux) and the notch effect. It was found that the multi axial stresses state and the high level of plastic strain in front of the notch were the key factors triggering crack initiation.
| Reference Key |
gabriele2017metalsbehavior
Use this key to autocite in the manuscript while using
SciMatic Manuscript Manager or Thesis Manager
|
|---|---|
| Authors | Fosca Di Gabriele;Anna Hojna;Michal Chocholousek;Jakub Klecka;Di Gabriele, Fosca;Hojna, Anna;Chocholousek, Michal;Klecka, Jakub; |
| Journal | metals |
| Year | 2017 |
| DOI |
10.3390/met7090342
|
| URL | |
| Keywords |
Citations
No citations found. To add a citation, contact the admin at info@scimatic.org
Comments
No comments yet. Be the first to comment on this article.