Integrated wood biorefinery: Improvements and tailor-made two-step strategies on hydrolysis techniques.
Clicks: 215
ID: 77295
2019
This study categorized different pretreatment methods into mild (below 120 °C), normal (120-200 °C) and extreme conditions (above 200 °C) for selective approach with efficient wood hydrolysis for direct market applications. The model two-step strategy of selective normal-hydrolysis: steam explosion (170 °C for 30 min) with concentrating normal-hydrolysis: organosolv at (160 °C for 20 min) on hard/softwood will delivery individual fractions of hemicellulose, lignin, and cellulose with recovery rate above 95%. The first step releases C5 sugars with a recovery rate of 80% followed by the second step for C6 sugars with 95% rate and direct use of reduced sugars into C5 and C6 value-added products. The categorized conditions will ease the selection of the pretreatment method for the wood type and model strategy will increase the hydrolysis rate with greater simplicity and validity. The integrated wood biorefinery with two-step treatment is an in-house and closed-loop with endless industrial applications.
Reference Key |
pachapur2019integratedbioresource
Use this key to autocite in the manuscript while using
SciMatic Manuscript Manager or Thesis Manager
|
---|---|
Authors | Pachapur, Vinayak Laxman;Kaur Brar, Satinder;Le Bihan, Yann; |
Journal | Bioresource technology |
Year | 2019 |
DOI | S0960-8524(19)31862-0 |
URL | |
Keywords |
Citations
No citations found. To add a citation, contact the admin at info@scimatic.org
Comments
No comments yet. Be the first to comment on this article.