Thermoelectric properties of high pressure synthesized lithium and calcium double-filled CoSb3
Clicks: 231
ID: 41132
2017
Lithium and calcium are inefficient filling elements of CoSb3 at ambient pressure, but show nice filling behavior under high pressure. In this work, we synthesized Li/Ca double-filled CoSb3 with high pressure synthesis method. The products show the skutterudite structure of Im3¯ symmetry. Thermoelectric properties were effectively enhanced through Li and Ca co-filling. For the optimal Li0.08Ca0.18Co4Sb12 sample, the power factor maintains a relatively high value over the whole measurement temperature range and peaks at 4700μWm−1K−2, meanwhile the lattice thermal conductivity is greatly suppressed, leading to a maximal ZT of 1.18 at 700 K. Current work demonstrates high pressure synthesis as an effective method to produce multiple elemental filled CoSb3 skutterudites.
Reference Key |
li2017thermoelectricaip
Use this key to autocite in the manuscript while using
SciMatic Manuscript Manager or Thesis Manager
|
---|---|
Authors | Li, Xiaohui;Kang, Yulong;Chen, Chen;Li, Jianghua;Zhang, Long;Yu, Fengrong;Yu, Dongli;Tian, Yongjun;Xu, Bo; |
Journal | aip advances |
Year | 2017 |
DOI | DOI not found |
URL | |
Keywords | Keywords not found |
Citations
No citations found. To add a citation, contact the admin at info@scimatic.org
Comments
No comments yet. Be the first to comment on this article.