Abstract
In order to improve the abrasion resistance of sport shoes rubber soles, 9 rubber compound formula has been observed, with variation in using of calcium silicate and aluminium silicate as filler and naphtenic oil as softener. The result of this research showed that the best value of the abrasion resistance was 0,0485 mm3/kgm and it fulfilled the requirements of Indonesian National Standard 0171-1987-A, Canvas shoes with rbber sole for sports. It constitutes the formula of 100 parts (by weight) of natural rubber, 25 parts of calcium silicate, 25 parts of aluminium silicate and 8 parts of naphtenic oil. The usage of 50 parts of calcium silicate and aluminium silicate fillers with 8-10 parts of naphtenic oil didn’t influence more on the hardness and its value fulfilled the requirements of Indonesian National Standard 0171-1987-A.
Reference Key
herminiwati1996penelitianmajalah Use this key to autocite in the manuscript while using SciMatic Manuscript Manager or Thesis Manager
Authors Herminiwati, Herminiwati;Setyaningsih, Any;Supriyadi, Adi Slamet;
Journal majalah kulit, karet, dan plastik
Year 1996
DOI DOI not found
URL
Keywords

Citations

No citations found. To add a citation, contact the admin at info@scimatic.org

No comments yet. Be the first to comment on this article.